SA长城系列耐火砖国内使用状况简表
SA Great Wall Series Refractories'Latest Reference List in China |
炉种
Furnace Type |
冶炼产品
Product |
使用单位
Company |
使用寿命与其他砖对比
Compared with Other Refractory Materials |
| 奥斯迈特炉Ausmelt |
铜
Copper |
中条山侯马冶炼厂
Zhongtiaoshan Houma Smelter |
SA-2L-AJ渣线砖长345mm、连续使用13个月后、残砖还有200mm左右长。进口砖只用2个多月、国产砖只用1个多月就没砖了。
SA-2L-AJ bricks on slag zone remained at around 200mm after 13 months operation,while the imported bricks can be used no more than 3 months and other domestic bricks no more than 2 months. |
锡
Tin |
云南锡业公司Yunnan Tin Co.,Ltd |
SA-1L-AJ渣线砖长345mm、连续使用24个月后、残砖还有160mm左右长、上部SA-3L-A砖345mm长使用48个月。而进口渣线砖只用4-7月局部就没砖了。
A-1L-AJ bricks on slag zone remained at around 160mm after 24 months operation;SA-3L-A bricks of 345mm at upper position were used for 48 months.The imported bricks were partially no bricks only after 4-7 months operation. |
铜
Copper |
铜陵金昌冶炼厂?
Tongling Jinchang Smelter |
SA-2L-AJ渣线砖长345mm、连续使用寿命达到18.5个月、残砖还有180mm左右长、还可以继续使用。
SA-2L-AJ bricks of 345mm on slag zone remained at around 180mm after 18.5 months operation and could be used longer. |
铜
Copper |
赤峰金剑铜业公司
Chifeng Jinjian Copper Co.,Ltd |
SA-2L-CJ渣线砖长450mm、连续使用10个多月、还在继续使用中、上部SA-3L-C砖长350mm、预计能用24个月。
SA-2L-CJ bricks of 450mm on slag zone have been using for more than 10 months and now still in operation;SA-3L-C bricks of 350mm at upper position were predicated to campaign for 24 months. |
铜
Copper |
葫芦岛锌厂
Huludao Zinc Smelter |
SA-2L-AJ砖、正在使用中。
A-2L-AJ bricks are being in operation. |
镍
Nickel |
吉林镍业股份公司?
Jilin Nickle |
SA-2L-AJ砖、正在使用当中。
A-2L-AJ bricks are being in operation. |
铜
Copper |
印度伯拉铜厂
Indian Birla Copper Smelter |
SA-2L-AJ渣线砖长350mm、炉龄比国外名牌镁铬质砖提高1倍寿命。
SA-2L-AJ bricks of 350mm on slag zone are two times of abroad famous brand Mg-Cr bricks. |
铜
Copper |
云铜集团凯通公司
Kaitong company of?Yunnan Copper Co.,Ltd |
SA-1L-AJ砖、正在施工中。
SA-1L-AJ bricks are being under construction. |
锡
Tin |
秘鲁明苏尔冶炼厂
Peru Minsur Smelter |
SA-1L-AJ渣线砖长350mm、炉龄比国外名牌镁铬质砖提高1倍寿命.
SA-1L-AJ bricks of 350mm on slag zone are two times of abroad famous brand Mg-Cr bricks in campaign. |
锡
Tin |
印尼锡业公司?
Indonesia Tin Co.,Ltd |
SA-2L-AJ渣线砖长350mm、炼锡渣已使用12个月、残砖180左右、上部使用24个月。
SA-2L-AJ bricks of 350mm on slag zone have been used for 12 months,the remained bricks are still 180mm long and the upper bricks 24 months. |
艾萨炉
Isa |
铜
Copper |
驰宏锌锗冶炼厂
Yunnan Chihong Zn and Ge Co.,Ltd |
SA-2L-AJ砖在渣线上部使用1年以上,还解决了镁铬砖一直过大膨胀问题。
A-2L-AJ bricks on upper slag zone have been used for more than 1 year,solving the problem of over expansion of Mg-Cr bricks. |
铜
Copper |
马来西亚冶炼厂
Malaysia Smelter |
SA-2L-AJ渣线与上部砖都在使用中,同时又解决了由于镁铬砖一直大量膨胀的问题。
SA-2L-AJ bricks on slag zone and on upper slag zone are in operation,solving the problem of over expansion of Mg-Cr bricks. |
| 反射炉Reverbratory Furnace |
锡
Tin |
云南锡业公司
Yunnan Tin Co.,Ltd |
SA-4L-CJ砖创造反射炉516.94天的云南锡业公司的历史最高记录,镁铬砖寿命只有5个月。
SA-4L-CJ bricks gained the longest campaign record of 516.94 days,while that of Mg-Cr bricks was only 5 months. |
挥发窑
Rotary Zinc Kiln |
锌
Zinc |
株洲冶炼厂
Zhuzhou Smelter |
SA-3L-BJ砖在5#锌挥发窑(该窑直径4.15m)上干砌已达到160多天,而铬渣砖,镁铬砖仅用80多天。
SA-3L-BJ bricks on 5# kiln(4.15m diameter)have been used for more than 160 days.chromate sludge bricks and Mg-Cr bricks can only campaign for 80 days. |
锌
Zinc |
河南豫光锌业有限公司
Henan Yuguang Zinc Limited |
SA-3L-BJ砖在4.15m直径的锌挥发回转窑已达到229天的平均寿命。
A-3L-BJ bricks on 4.15 diameter rotary zinc kiln have reached the average service life of 229 days. |
锌
Zinc |
蒙自矿冶股份公司
Mengzi Mining and Metallurgy Limited |
SA-3L-BJ砖在4.15m直径的锌挥发回转窑创造了300天的挥发窑记录。
SA-3L-BJ bricks on 4.15m diameter rotary zinc kiln reached a campaign of 300 days. |
锌
Zinc |
广西南方冶炼厂
Guangxi Nanfang Smelter |
SA-3L-CJ砖在4.3m直径挥发窑正在使用中。
A-3L-CJ bricks on 4.3m diameter rotary zinc kiln are being in operation. |
锌
Zinc |
来宾冶炼厂
Guangxi Laibin Smelter |
SA-3L-BJ砖在3.45m挥发窑上达到了395天的使用寿命,创造了回转窑行业该窑直径的最高窑寿记录。
SA-3L-BJ bricks on 3.45 diameter rotary zinc kiln have reached a campaign of 395 days.Our products had broken the longest campaign record in the circle of rotary kiln of this size. |
锌
Zinc |
广西金河冶炼厂
Guangxi Jinhe Smelter |
SA-3L-BJ砖在3.45m直径的锌挥发回转窑达到一年以上的使用寿命。
SA-3L-BJ bricks on 3.45 diameter rotary zinc kiln have reached a campaign more than 1year. |
锌
Zinc |
广西龙城化工
Guangxi Longcheng Chemical Plant |
SA-4L-BJ砖在2.4m直径锌挥发窑寿命超过了铬渣砖一倍。
A-4L-BJ bricks on 2.4m diameter rotary zinc kiln are two times of chromate sludge bricks in campaign. |
锌
Zinc |
秘鲁锌业公司
Peru Zinc Co.,Ltd |
SA-2L-AJ砖在4.3m直径锌挥发窑寿命超过了260天。
SA-2L-AJ bricks on 4.3m diameter rotary zinc kiln have surpassed 260 days. |
转炉
Converter |
镍
Nickle |
金川集团
Jinchuan Group Ltd |
SA-3L-BJ风眼及风眼区砖达100炉左右,而镁铬砖仅用50-60炉。
A-3L-BJ bricks on tuyere and tuyere zone reached 100± heats,while that of Mg-Cr only 50-60 heats. |
镍
Nickle |
吉林镍业公司
Jilin Nikcle Co.,Ltd |
SA-3L-BJ风眼及风眼区砖,比镁铬砖高出一倍。
A-3L-BJ bricks on tuyere and tuyere zone is two times of Mg-Cr bricks. |
闪速炉
Flash Furnace |
铜
Copper |
山东祥光铜业公司
Shandong Xiangguang Copper Co.,Ltd |
SA-1L-AJ用在闪速炉放出口比进口镁铬砖高出一倍还多。
A-1L-AJ bricks on outlet are more than two times of imported Mg-Cr bricks in service life. |
铜
Copper |
金隆铜业公司
Jinlong Copper Co.,Ltd |
SA-1L-AJ使用在熔池部位1年半之久,并还在继续使用。
A-1L-AJ bricks on smelting bath lasted for 1 year and a half and now still in use. |
富氧底吹炉
SKS Furnace |
铅
Lead |
河南豫光金铅集团
Henan Yuguang Gold&Lead Co.,Ltd |
SA-T2L-AJ氧枪砖达到进口镁铬砖水平,成功取代进口转。
A-T2L-AJ bricks on oxygen lance is the same as imported Mg-Cr bricks.Our bricks successfully replace the imported bricks. |
铅
Lead |
铜冠贵池冶炼厂
Tongguan Guichi Smelter |
SA-T2L-AJ氧枪砖使用效果与进口镁铬砖相比,已超过其使用寿命。
A-T2L-AJ bricks on oxygen lance have surpassed the service life of imported Mg-Cr bricks. |
铅
Lead |
水口山冶炼厂
Shuikoushan Smelter |
SA-T2L-AJ成功取代进口转,使用效果比进口砖还高。
A-T2L-AJ bricks on oxygen lance successfully replace the imported bricks and the result is much better than those imported. |
铅
Lead |
云南祥云飞龙公司
Yunnan Xiangyun Feilong Limited |
SA-T2L-AJ氧枪砖已达到并超过进口镁铬砖水平。
A-T2L-AJ bricks on oxygen lance have reached the level of the imported Mg-Cr bricks in service life. |
铅
Lead |
河南万洋公司
Henan Wanyang Limited |
SA-T2L-AJ氧枪砖已达到并超过进口镁铬砖水平。
A-T2L-AJ bricks on oxygen lance have reached the level of the imported Mg-Cr bricks in service life. |
铜
Copper |
飞尚铜业公司
Feishang Copper Limited |
SA-T2L-AJ氧枪砖已达到并超过进口镁铬砖水平。
A-T2L-AJ bricks on oxygen lance have reached the level of the imported Mg-Cr bricks in service life. |
铅
Lead |
河南灵宝新凌公司
Henan Lingbao Xinling Co.,Ltd |
SA-T2L-AJ目前使用效果良好。
SA-T2L-AJ bricks now are in good operation. |
白银炉
Baiyin Furnace |
铜
Copper |
甘肃白银公司
Gansu Baiyin Co., Ltd |
SA-2L-AJ风眼砖开炉十个月后,残砖还剩200mm。SA-5L-BJ炉顶砖达10个月、镁铬砖仅用2-3个月。
SA-2L-AJ bricks on tuyere still remained 200mm after 10months operation; SA-5L-BJ bricks on furnace roof reached a campaign of 10 months,2-3months that of Mg-Cr bricks. |
阳极炉
Anode Furnace |
铜
Copper |
山东祥光铜业公司
Shandong Xiangguang Copper Co.,Ltd |
SA-2L-BJ风口砖比进口镁铬砖提高一倍左右。
SA-2L-BJ bricks on tuyere is two times of imported Mg-Cr bricks. |
铜
Copper |
铜陵金隆公司
Tongling Jinlong Co.,Ltd |
SA-2L-BJ风眼砖使用达210天,半再结合镁铬砖只用60天。
SA-2L-BJ bricks on tuyere campaigned for 210 days,while semi-bonded Mg-Cr bricks lasts only 60 days. |
铜
Copper |
富春江冶炼厂
Fuchunjiang Smelter |
SA-4L-BJ渣线砖使用176炉,比镁铬砖高出一倍还多。
A-4L-BJ bricks on slag zone campaigned 176 heats,that is two times more than Mg-Cr bricks. |
电炉
Electric Furnace |
锌
Zinc |
陕西旬阳柯达冶炼厂
Shanxi Xunyang Keda Smelter |
SA-4L-BJ渣线砖已用12个月,比铬渣砖延长5个月。
SA-4L-BJ bricks on slag zone have been used for 12 months,5 months longer than chromate sludge bricks. |
锌
Zinc |
山西运城关铝冶炼厂
Shanxi Yuncheng Guanlv Smelter |
SA-4L-BJ渣线砖已用12个月以上。
A-4L-BJ bricks on slag zone have campaigned for more than 12 months. |
锌
Zinc |
四川昌达冶炼厂
Sichuan Changda Smelter |
SA-3L-CJ渣线砖比铬渣砖延长4个月寿命。
A-3L-CJ bricks on slag zone is 4month longer than chromate sludge bricks. |
锌
Zinc |
陕西宝鸡锌业有限公司
Shanxi Baoji Zinc Co.,Ltd |
SA-4L-CJ渣线砖已用8个多月,比铬渣砖延长4个月。
A-4L-CJ bricks on slag zone have been used for 8 months,4 month longer than chromate sludge bricks. |
锌
Zinc |
陕西宝鸡恒锌业公司
Shanxi Baojiheng Zinc Co.,Ltd |
SA-4L-BJ渣线砖已用13个月,比铬渣砖延长5个月。
A-4L-BJ bricks on slag zone have been used for 13 months,5 months longer than chromate sludge bricks. |
铜钴镍 Cu&Co balt&N ickle
|
刚果金
The democratic Republic of the Congo |
在新材质的冶炼使用上取得了突破。
breakthrough on new material smelting. |
贫化电炉
Electric Cleaning Furnace |
铜
Copper |
中条山侯马冶炼厂
Zhongtiaoshan Houma Smelter |
SA-3L-AJ砖从2001年使用,目前已达到8年之多,还在继续使用。
SA-3L-AJ bricks have been in operation for more than 8 years since 2001,and now still in use. |
铜
Copper |
山东东营铜冶炼厂
Shandong Dongying Copper Smelter |
SA-3L-AJ渣线砖正在使用中。
SA-3L-AJ bricks on slag zone are in operation. |
铜
Copper |
赤峰金剑铜业公司
Chifeng Jinjian Copper Co.,Ltd |
SA-3L-AJ砖已使用18个月仍在继续使用中。
SA-3L-AJ bricks have campaigned for 18 months and could be used longer. |
电热前床
Electro-thermol-bed |
铅
Lead |
河南豫光金铅公司
Henan Yuguang Gold&Lead Co.,Ltd |
一直使用SA-4L-CJ耐火砖,使用3年半效果显著,得到厂家认可。
Our SA-4L-CJ bricks have be used for 3 year and a half and were approved by the company. |
铅
Lead |
驰宏锌锗曲靖冶炼厂
Qujing Chihong Zinc&Ge Smelter |
目前也达到3年半的使用效果。
ur pruducts have successfully campaigned for 3 years and a half. |
铅
Lead |
云南祥云飞龙公司
Yunnan Xiangyun Feilong Co., Ltd |
目前还在使用中。
Our bricks are being in operation now. |
烟化炉
Smokify Furnace |
锡
Tin |
云南锡业公司
Yunnan Tin Co.,Ltd |
原来铬镁砖2个月的使用寿命,改用SA-3T-B砖提高到6个月以上。
SA-3T-B bricks campaigned 6 months longer than the original Cr-Mg bricks which can only campaign 2 months. |
锡
Tin |
个旧新冶
Gejiu Xinye Co., Ltd |
原来铬镁砖2个月的使用寿命,改用SA-3T-B砖提高到6个月更换一次。
A-3T-B bricks campaigned 6 months longer than the original Cr-Mg bricks which can only campaign 2 months. |
铅
Lead |
驰宏锌锗冶炼厂
Chihong Zinc&Ge Smelter |
目前也使用效果良好。
Our bricks works well right now. |